Hymix Pump 100 MPa - 53% Indicative Cement Replacement - Fly Ash/GGBFS/Silica Fume - Sydney

Concrete in-situ 100Mpa
Australia
LCM-3DSupplier
HAPL
Hymix Australia Pty Ltd
Specifications
Compressive-strength100 MPaDensity2415 kg/m3
kg CO2-eq./m3
Info
A1-A3449.00A1-A2-A3-A40.57A513.10B1-7.07B20.00B30.00B40.00B50.00B60.00B70.00C18.99C28.64C33.73C4-2.60D-14.20
EPD
Certifications
ISO14020
ISO14025
ISO14044
EN15804:A2
EN16757+A0
EN16908+A0