Hymix Post-Tensioned 40 MPa (25 MPa @ 3 Days) Generic Concrete - Sydney

Concrete in-situ 40Mpa
Australia
LCM-5ESupplier
HAPL
Hymix Australia Pty Ltd
Description
Post-Tensioned Slab
Specifications
Compressive-strength40 MPaDensity2414.4 kg/m3Recycling-rate-at-end-of-life78 %
kg CO2-eq./m3
Info
A1-A3366.00A1-A2-A3-A45.17A512.80B1-7.35B20.00B30.00B40.00B50.00B60.00B70.00C19.64C210.50C33.24C43.33D-13.60
EPD
Certifications
ISO14025
EN15804:A2
EN16757+A0