Hymix Piling 40 MPa HyLo-50 Sunshine Coast

Concrete in-situ 40Mpa
Australia
LCM-1CSupplier
HAPL
Hymix Australia Pty Ltd
Description
Piling concrete with a compressive strength of 40 MPa, designed for piling applications. Manufactured in Sunshine Coast, Queensland.
Specifications
Density2290.4 kg/m3Compressive-strength40 MPa
kg CO2-eq./m3
Info
A1-A3207.00A1-A2-A3-A44.90A511.30B1-3.56B20.00B30.00B40.00B50.00B60.00B70.00C19.64C29.95C34.25C43.16D-12.90
EPD
Certifications
ISO14025
ISO14044
EN15804+A2