Our platform is optimised for desktop. Please use a desktop browser to access the full features.

Heidelberg Materials Post-tensioned 50 MPa (22 MPa @ 2 days) Concrete - Western Australia, AU

Product photo
Concrete in-situ 50MpaAustraliaAustralia
LCM-5F

Supplier

HMAPL
Heidelberg Materials Australia Pty Ltd

Specifications

Density2411 kg/m3Service life50 yearsConcrete applicationpre_and_post_tensionCompressive strength mpa50 MPa

kg CO2-eq./m3

Info
A1-A3462.00A1-A2-A3-A45.16A513.80B1-7.86B2-B3-B4-B5-B6-B7-C19.64C210.50C33.18C4-5.61D-14.20

EPD

EPDView documentVersion1Emitted inMay 2, 2025Valid untilMay 2, 2030

Certifications

ISO 14025