Heidelberg Materials Piling 32 MPa Enrich-50 Sydney

Concrete in-situ 32Mpa
Australia
LCM-1CSupplier
HMAPL
Heidelberg Materials Australia Pty Ltd
Description
Piling concrete mix with 32 MPa compressive strength, Enrich-50 formulation, suitable for piling applications.
Specifications
Density2371.1 kg/m3Compressive-strength32 MPa
kg CO2-eq./m3
Info
A1-A3187.00A1-A2-A3-A45.08A511.10B1-B2-B3-B4-B5-B6-B7-C19.64C210.30C34.32C43.27D-13.40