CoreMasta 25 MPa Blockfill Sunshine Coast

Concrete in-situ 25Mpa
Australia
LCM-2CSupplier
HMAPL
Heidelberg Materials Australia Pty Ltd
Description
CoreMasta 25 MPa concrete mix designed for blockfill applications with a density of 2112 kg/m3 and compressive strength of 25 MPa.
Specifications
Density2112 kg/m3Compressive-strength25 MPa
kg CO2-eq./m3
Info
A1-A3178.00A1-A2-A3-A44.52A511.00B1-B2-B3-B4-B5-B6-B7-C19.64C29.17C33.68C42.91D-11.90
EPD
Certifications
ISO14020
ISO14025
ISO14044
EN15804+A2
EN16908